Suitability study of jute-epoxy composite laminate for low and high velocity impact applications

机译:黄麻环氧复合层压材料对低速和高速冲击应用的适用性研究

获取原文

摘要

This paper discusses the effect of thickness on the energy absorbing ability of the jute-epoxy (JE) laminate under low velocity and high velocity impact conditions. In the present analysis, a parametric study has been carried out choosing three different thickness values of laminate (6 mm, 8mm and 10 mm) and four different velocities each under low (2m/s, 4m/s, 6m/s and 8m/s) and high velocity (100 m/s, 150 m/s, 200 m/s and 250 m/s) impact conditions. A Damage behavior study has been carried out under both low and high velocity impacts to assess the suitable condition of application for JE laminate. It is found that, the energy absorbing ability of laminate increases with increasing laminate thickness and impact velocity, especially at higher values of impact velocity of the chosen regime. The outcome of the study of damage behavior under low and high velocity impact shows that JE laminate is suitable for low velocity impact applications rather than high velocity impact applications.
机译:本文讨论了厚度对低速度和高速冲击条件下黄麻 - 环氧(JE)层压板的能量吸收能力的影响。在本分析中,已经进行了参数研究,选择了三种不同厚度值的层压板(6mm,8mm和10mm)和每个低于低(2m / s,4m / s,6m / s和8m /)的四种不同速度的厚度值。 S)和高速(100 m / s,150 m / s,200 m / s和250 m / s)的影响条件。在低速和高速冲击下进行了损伤行为研究,以评估JE层压板的合适施用条件。结果发现,层压材料的能量吸收能力随着层压厚度和冲击速度的增加而增加,特别是在所选方案的冲击速度的较高值下。低速和高速冲击下损伤行为研究的结果表明,JE层压板适用于低速冲击应用而不是高速冲击应用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号