Microstructure, Densification and Mechanical Properties of TiB_2-TiC-NiAl Ceramic-Based Composite

机译:基于TIB_2-TIC-nial陶瓷复合材料的微观结构,致密化和力学性能

获取原文

摘要

By adjusting mass fraction of Ni-Al composite additive in Ti-B_4C primary system, a series of TiB_2-based ceramic composites were prepared by combustion synthesis in high gravity field. Because the adiabatic temperature of the whole reaction system maintained a constant in the presence of mass fraction of Ni-Al additive smaller than 18.55%, increasing mass fraction of Ni-Al additive to be 15% brought about the improved homogeneity in refined microstructure of the enhanced-densification TiB_2-based composite, so flexural strength and fracture toughness of the ceramic composite increased simultaneously due to the enhanced self-toughening mechanisms contributed by a number of fine TiB_2 platelets.
机译:通过调节Ti-B_4C初级系统中Ni-Al复合添加剂的质量分数,通过高重物燃烧合成制备一系列Tib_2陶瓷复合材料。 由于整个反应体系的绝热温度在镍酯添加剂的质量分数存在下保持恒定,所以少于18.55%,增加Ni-Al添加剂的质量分数为15%,所以提高了精细组织的改善的均匀性 增强致密化Tib_2基复合材料,因此由于多种精细的Tib_2血小板贡献的增强的自增韧机制,陶瓷复合材料的弯曲强度和断裂韧性同时增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号