首页> 外文会议>Annual Meeting on Testing and Evaluation of Advanced Materials >Microstructure, Densification and Mechanical Properties of TiB_2-TiC-NiAl Ceramic-Based Composite
【24h】

Microstructure, Densification and Mechanical Properties of TiB_2-TiC-NiAl Ceramic-Based Composite

机译:基于TIB_2-TIC-nial陶瓷复合材料的微观结构,致密化和力学性能

获取原文

摘要

By adjusting mass fraction of Ni-Al composite additive in Ti-B_4C primary system, a series of TiB_2-based ceramic composites were prepared by combustion synthesis in high gravity field. Because the adiabatic temperature of the whole reaction system maintained a constant in the presence of mass fraction of Ni-Al additive smaller than 18.55%, increasing mass fraction of Ni-Al additive to be 15% brought about the improved homogeneity in refined microstructure of the enhanced-densification TiB_2-based composite, so flexural strength and fracture toughness of the ceramic composite increased simultaneously due to the enhanced self-toughening mechanisms contributed by a number of fine TiB_2 platelets.
机译:通过在Ti-B_4C初级系统中调节Ni-Al复合添加剂的质量分数,通过高重物燃烧合成制备一系列TIB_2的陶瓷复合材料。由于整个反应体系的绝热温度在大于18.55%的镍酯添加剂的质量分数存在下保持恒定,因此将Ni-Al添加剂的质量分数增加为15%,所以提高了精磨微观结构的提高均匀性增强致密化Tib_2基复合材料,因此由于多种精细Tib_2血小板贡献的增强的自增韧机制,陶瓷复合材料的弯曲强度和断裂韧性同时增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号