Asphalt rubber binders are produced by mixing crumb rubber obtained from ground used tires with a straight run binder at high temperatures during a period of time named as digestion time. This is one of many variables that influence the physical properties of asphalt rubber produced by wet process. Thus, the objective of this paper is to evaluate how many mechanical properties of gap-graded hot mixes produced with asphalt rubber binder are influenced by the digestion time used to produce this modified binder. The asphalt rubber binders were produced by incorporating 21% in weight of crumb rubber into a straight run binder at 210°C. The digestion times used were 60 and 300 minutes. These asphalt rubber binders were used to produce gap-graded hot mixes which were submitted to tensile strength, fatigue life, resilient modulus and permanent deformation tests. The results show that the increase of digestion time used to produce asphalt rubber binders led to a decrease of tensile strength, resilient modulus and permanent deformation. However, there was a significantly increase of fatigue life of asphalt hot mixes studied.
机译:沥青橡胶粘合剂是通过在一段时间内的高温下与直线粘合剂的地面使用的碎屑橡胶混合使用的碎屑橡胶制备。这是众多变量之一,影响湿法生产的沥青橡胶物理性质的变量之一。因此,本文的目的是评估用沥青橡胶粘合剂制备的间隙梯度热混合物的机械性能有多少受用于生产该改性粘合剂的消化时间。通过在210℃下将21%的碎屑橡胶掺入直线运行粘合剂中,制备沥青橡胶粘合剂。使用的消化时间为60和300分钟。这些沥青橡胶粘合剂用于产生间隙梯度的热混合物,其提交拉伸强度,疲劳寿命,弹性模量和永久变形试验。结果表明,用于生产沥青橡胶粘合剂的消化时间的增加导致拉伸强度,弹性模量和永久变形的降低。然而,研究了沥青热混合物的疲劳寿命显着增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号