Aging Studies of Pu-238 and -239 Containing Calcium Phosphate Ceramic Waste-forms

机译:PU-238和-239含有磷酸钙陶瓷废物 - 形式的衰老研究

获取原文

摘要

A calcium phosphate ceramic waste-form has been developed at AWE for the immobilisation of chloride containing wastes arising from the pyrochemical reprocessing of plutonium. In order to determine the long term durability of the waste-form, aging trials have been carried out at PNNL. Ceramics were prepared using Pu-239 and -238, these were characterised by PXRD at regular intervals and Single Pass Flow Through (SPFT) tests after approximately 5 yrs. While XRD indicated some loss of crystallinity in the Pu-238 samples after exposure to 2.8 × 10~(18) α decays, SPFT tests indicated that accelerated aging had not had a detrimental effect on the durability of Pu-238 samples compared to Pu-239 waste-forms.
机译:磷酸钙陶瓷废物形式已经在敬畏中开发,用于固定含有钚的热化学再加工引起的氯化物的氯化物。为了确定废物形式的长期耐久性,在PNN1进行了衰老试验。使用PU-239和-238制备陶瓷,其特征在于PXRD以规则的间隔,并通过(SPFT)通过(SPFT)测试在约5年后进行。虽然在暴露于2.8×10〜(18)α衰减后,XRD在PU-238样品中表明了一些结晶度损失,但SPFT试验表明,与PU - 相比,加速老化对PU-238样品的耐久性没有不利影响239废物形式。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号