Y_2O_2S:Eu~(3+) was prepared by the flux method which is different from conventional solid state reaction and has many advantages over the conventional method in terms of ease of preparation and yield also. In this paper we have reported the crystal structure, XRD and method of preparation of Y_2O_2S:Eu~(3+) along with Eu~(3+) mechanism of emission and excitation with reference to solid state lighting. In the emission spectra, the strongest red-emission lines at 626 and 616 nm are due to transition from ~5D_0 → ~7F_2 level. The stronger emission at λem=626 nm confirms the formation of the oxysulfide host. We also made a comparison of our prepared sample with commercial sample from NICHIA Corporation Japan in terms of PL intensity which results that our sample is equally intense as that of NICHIA's sample. It is suggested that these characteristics can be useful for obtaining a low cost, red phosphor for the solid state lighting using near UV LED.
机译:Y_2O_2S:Eu〜(3+)由与常规固态反应不同的助熔剂方法制备,并且在易于制备和产率方面具有与常规方法相比的许多优点。在本文中,我们已经报道了Y_2O_2S的晶体结构,XRD和制备方法:EU〜(3+)以及欧盟〜(3+)的发射机制,并参考固态照明。在发射光谱中,626和616nm处的最强的红色发射线是由于从〜5d_0→〜7f_2级​​的转变。 λem= 626nm处的较强发射证实了氧硫化物宿主的形成。我们还将我们的准备样品与来自Nichia Corporation Japan的商业样本的比较,从PL强度方面,这导致我们的样本与Nichia的样本相同强烈。建议这些特性对于使用近UV LED获得用于固态照明的低成本,红色磷光体是有用的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号