Quantitative Analysis of Core Binding Factor 1 (Cbfa1) and Osteocalcin in C2C12 Cells Induced by Ca/P Ceramics in vitro

机译:核心结合因子1(CBFA1)和CA / P陶瓷在体外C2C12细胞中的核心结合因子和骨钙的定量分析

获取原文

摘要

The mRNA expression of Cbfa1 and osteocalcin gene induced by calcium phosphate ceramics (Ca/P) were quantitative analyzed according to real-time RT-PCR method in this work. C2C12 cells were co-culture with four kinds of porous Ca/P ceramics for 2 and 5d without adding other growth factors. The four kinds of Ca/P ceramics were pure hydroxyapatite (HA) sintered at 1250°C and HA/TCP with a ratio of 60/40 sintered at 1100°C (HT1), 1200°C (HT2) and 1250°C (HT3) respectively. Real-time RT-PCR analysis found the Ca/P ceramics induced positive expression of Cbfa1 and osteocalcin in C2C12 cells, After 5 days culture, Cbfa1 and osteocalcin showed obvious higher expression compared with that in 2 days. Cbfa1 and osteocalcin expression in BCP was much higher than HA, and the expression level of osteocalcin was HT1>HT2>HT3>HA. Our results showed that Ca/P ceramics alone were sufficient to induce C2C12 cells to osteoblastic differentiation and the sinter temperature and phase composition of Ca/P ceramics could affect their osteoindctive capacity significantly.
机译:磷酸钙陶瓷(CA / P)诱导的CBFA1和骨钙素基因的mRNA表达根据本工作中的实时RT-PCR方法进行定量分析。 C2C12细胞与2种多孔Ca / P陶瓷共同培养,2和5D,不添加其他生长因子。 CA / P陶瓷的四种CA / P陶瓷(HA)在1250℃和HA / TCP下烧结,具有60/40烧结在1100℃(HT1),1200℃(HT2)和1250℃( HT3)分别。实时RT-PCR分析发现CA / P陶瓷在C2C12细胞中诱导CBFA1和骨钙蛋白的阳性表达,在5天培养后,CBFA1和骨钙素显示出明显更高的表达,与2天相比。 BCP中的CBFA1和骨钙素表达得多高于HA,骨钙素的表达水平为HT1> HT2> HA。我们的研究结果表明,单独的CA / P陶瓷足以诱导C2C12细胞对成骨细胞分化,并且CA / P陶瓷的烧结温度和相位组成可能会显着影响其骨导管。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号