The mRNA expression of Cbfa1 and osteocalcin gene induced by calcium phosphate ceramics (Ca/P) were quantitative analyzed according to real-time RT-PCR method in this work. C2C12 cells were co-culture with four kinds of porous Ca/P ceramics for 2 and 5d without adding other growth factors. The four kinds of Ca/P ceramics were pure hydroxyapatite (HA) sintered at 1250℃ and HA/TCP with a ratio of 60/40 sintered at 1100℃ (HT1), 1200℃ (HT2) and 1250℃ (HT3) respectively. Real-time RT-PCR analysis found the Ca/P ceramics induced positive expression of Cbfa1 and osteocalcin in C2C12 cells, After 5 days culture, Cbfa1 and osteocalcin showed obvious higher expression compared with that in 2 days. Cbfa1 and osteocalcin expression in BCP was much higher than HA, and the expression level of osteocalcin was HT1>HT2>HT3>HA. Our results showed that Ca/P ceramics alone were sufficient to induce C2C12 cells to osteoblastic differentiation and the sinter temperature and phase composition of Ca/P ceramics could affect their osteoindctive capacity significantly.
机译:根据实时RT-PCR方法,定量分析磷酸钙陶瓷(Ca / P)诱导的Cbfa1和骨钙素基因的mRNA表达。在不添加其他生长因子的情况下,将C2C12细胞与四种多孔Ca / P陶瓷共培养2天和5天。四种Ca / P陶瓷分别是在1250℃烧结的纯羟基磷灰石(HA)和在1100℃(HT1),在1200℃(HT2)和1250℃(HT3)烧结的比例为60/40的HA / TCP。实时RT-PCR分析发现,Ca / P陶瓷诱导的C2C12细胞中Cbfa1和骨钙蛋白的阳性表达。培养5天后,Cbfa1和骨钙素的表达明显高于2天。 BCP中Cbfa1和骨钙素的表达远高于HA,骨钙素的表达水平为HT1> HT2> HT3> HA。我们的结果表明,仅Ca / P陶瓷足以诱导C2C12细胞成骨细胞分化,并且Ca / P陶瓷的烧结温度和相组成可能会显着影响其成骨能力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号