Corrosion under insulation (CUI) has been a continuous challenge for on- and off-shore installations, requiring continuous focus on maintenance work. Pilot scale accelerated testing has been performed to study and evaluate the effects of CUI on different coating systems and service conditions. A test loop has been constructed, where 115 mm o.d. pipe spools were combined in a loop which is internally heated using steam. The coated and insulated pipe spools were exposed at controlled internal temperatures and intermittently wetted by fresh seawater. Two test lines with 8 pipe spools have been run in parallel.Different aspects of CUI, including methods of steel pretreatment, coating application conditions, coating types and insulation design have been studied. Special focus has been on high temperature service conditions and the effect of moist and intermittently wet condition. High temperature coatings have been compared with a traditional coating system and thermally sprayed aluminum coating. The effect of coating application during service with steel temperatures up to 150°C has been studied.Due to the harsh exposure conditions, both tested coating systems were heavily degraded and a fair comparison of the coating systems is difficult. A positive effect of distance insulation was the most significant result from the test, and both tested coating systems showed markedly improved quality using distance insulation. The different application temperatures showed significant differences, and the results were in general better for the coatings applied at ambient conditions. Only minor differences were observed between the different steel pre-treatment methods.
机译:绝缘下的腐蚀(CUI)对岸上和离岸装置来说是一个持续的挑战,需要连续关注维护工作。已经进行了试验规范加速测试,以研究和评估CUI对不同涂层系统和服务条件的影响。建造了一个测试回路,其中115 mm O.D.管道轴在环内加热的环中混合在一起。涂覆的和绝缘管道阀芯暴露在受控的内部温度下,并受新鲜海水间歇地润湿。具有8个管道线轴的两个测试线已平行运行。 已经研究了CUI的不同方面,包括钢预处理,涂料施用条件,涂料和绝缘设计的方法。特别焦点一直在高温服务条件和湿润和间歇性湿润的效果。将高温涂层与传统涂层系统和热喷涂的铝涂层进行比较。研究了涂料在钢筋膜中涂层应用高达150°C的效果。 由于苛刻的曝光条件,两个测试的涂料系统都很严重降低,并且难以进行涂层系统的公平比较。距离绝缘的积极效果是测试中最重要的结果,并且两种测试系统都显示出使用距离绝缘的质量明显提高。不同的应用温度显示出显着的差异,结果一般更好地涂覆在环境条件下的涂层。在不同的钢预处理方法之间仅观察到微小差异。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号