This article describes the problems of deterioration of the quality of processed raw materials due to depletion of mineral resources. It is proposed to use nitric acid for the processing of complex refractory low-grade concentrates containing non-ferrous and noble metals. It was found that the studied concentrate contains: sphalerite (26.9%), pyrite (22.0%), chalcopyrite (19.9%), silica (13.9%), alumina (5.5%), galena (1.7%), oxidized forms of iron (Fe_2O_3) (12%). Gold and silver are associated with sulfide minerals. Typical reactions of interaction of these minerals with nitric acid are considered. A sufficiently high thermodynamic probability of these reactions in a wide temperature range is established. With the use of mathematical methods, the optimal conditions of the process of nitric acid leaching are selected: the ratio of L:S = 5:1; the concentration of nitric acid 10 mol/L; the duration of the process is 60 minutes. In this case, the extraction of copper, zinc, iron and sulfur into the solution was 99.00%, 99.84% 98.60%, 88.51%, respectively.
机译:本文介绍了由于矿产资源消耗导致加工原料质量恶化的问题。提出使用硝酸来加工含有有色金属和贵金属的复杂耐火低级浓缩物。发现研究的浓缩物含有:闪锌矿(26.9%),黄铁矿(22.0%),黄铜矿(19.9%),二氧化硅(13.9%),氧化铝(5.5%),Galena(1.7%),氧化形式的铁( fe_2o_3)(12%)。金银与硫化物矿物质有关。考虑这些矿物与硝酸相互作用的典型反应。建立了宽温度范围内这些反应的足够高的热力学概率。利用数学方法的使用,选择硝酸浸出过程的最佳条件:L:S = 5:1的比例;硝酸10mol / l的浓度;过程的持续时间为60分钟。在这种情况下,将铜,锌,熨斗和硫的提取分别为99.00%,99.84%98.60%,88.51%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号