Pretreatments and Their Durability in Extrusion Coated Products

机译:挤压涂层产品中的预处理及其耐久性

获取原文

摘要

1. Good adhesion needs also chemical bonding 2. With LDPE this means that suitable oxidation carbonyi (groups) needed 3. Melt temperature is most important (slides 12,13,14 and 16) 4. Line speed (time in the air gap) is important, too (slide 15) 5. The oxidation occurs in the air gap (nip distance and line speed) (slide 11) 6. All parameters that increase aldehydes, ketones, esters increases the bond (slide 5) 7. Ozone oxidized molten polymer in right side, but is not enough for acceptable adhesion with difficult substrates (slides 15 and 18) 8. Adhesion values depends on substrate but also measurement method effects (slides 17 and 18) 9. With ozone treatment lower melt temperature can be run to reach enough chemical bonding (slides 16 and 17) 10. Best adhesion can be achieved when substrate is pretreated (Corona, Flame or Plasma) and ozone also used (slides 13 and 23) 11. No big differences between Corona or Flame (slides 13 and 14) 12. No better if all (Oz+C+F) are used (slides 13 and 14).
机译:1.良好的粘合力还需要化学键合2.使用LDPE,这意味着需要合适的氧化碳(基团)3.熔融温度最为重要(幻灯片12、13、14和16)4.线速度(气隙中的时间)同样重要的是(幻灯片15)5.空气间隙中发生氧化(压区距离和线速度)(幻灯片11)6.增加醛,酮,酯的所有参数都会增加键(幻灯片5)7.臭氧被氧化熔融的聚合物在右侧,但不足以与困难的基材(幻灯片15和18)保持可接受的粘合力。8粘合力值取决于基材,但还取决于测量方法的效果(幻灯片17和18)9.使用臭氧处理,可以降低熔体温度。运行以达到足够的化学键合(幻灯片16和17)。10.对基材进行预处理(电晕,火焰或等离子)并且还使用臭氧(幻灯片13和23)时,可以获得最佳的粘合力。11.电晕或火焰之间没有太大差异(幻灯片13和14)12.如果全部使用(Oz + C + F)也不会更好(幻灯片13和d 14)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号