1. Good adhesion needs also chemical bonding 2. With LDPE this means that suitable oxidation carbonyi (groups) needed 3. Melt temperature is most important (slides 12,13,14 and 16) 4. Line speed (time in the air gap) is important, too (slide 15) 5. The oxidation occurs in the air gap (nip distance and line speed) (slide 11) 6. All parameters that increase aldehydes, ketones, esters increases the bond (slide 5) 7. Ozone oxidized molten polymer in right side, but is not enough for acceptable adhesion with difficult substrates (slides 15 and 18) 8. Adhesion values depends on substrate but also measurement method effects (slides 17 and 18) 9. With ozone treatment lower melt temperature can be run to reach enough chemical bonding (slides 16 and 17) 10. Best adhesion can be achieved when substrate is pretreated (Corona, Flame or Plasma) and ozone also used (slides 13 and 23) 11. No big differences between Corona or Flame (slides 13 and 14) 12. No better if all (Oz+C+F) are used (slides 13 and 14).
机译:1.良好的附着力还需要化学键合2.使用LDPE,这意味着所需的合适氧化碳酸碱(组)需要3.熔体温度最重要(滑动12,13,14和16)。线速度(气隙中的时间)很重要(滑动15)5。氧化发生在气隙(辊隙距离和线速)(滑动率11)6中发生氧化。增加醛,酮,酯的所有参数增加键(滑动5)7.臭氧氧化右侧的熔融聚合物,但是对于难以接受的粘合性,难以与困难的基板(滑动件15和18)8。粘合值取决于基板,而且还取决于衬底,而且测量方法效果(幻灯片17和18)9。具有臭氧处理较低的熔体温度运行以达到足够的化学粘合(滑动率16和17)10。当衬底预处理(电晕,火焰或血浆)和臭氧(幻灯片13和23)11中,可以实现最佳粘合力(滑动13和23)11.电晕或火焰之间没有大的差异(幻灯片13和14)12。如果使用全部(oz + c + f),则不更好地(滑动13a D 14)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号