OPTIMAL PRECIPITATION HARDENING CONDITIONS IN LEAD BASE ANODES FOR COPPER ELECTROWINNING

机译:铜电解镀铅基阳极中的最佳析出硬化条件

获取原文

摘要

The suitable yield stress of Pb-0.07%Ca-1.3%Sn anodes of 6 mm thickness for copper electrowinning is achieved by means of deformation and precipitation hardening processes, being its useful life dependant of this yield stress. In such sense the objective of the present work is to optimize the precipitation hardening, finding for this purpose the best cooling conditions of the anodes in the molds and of the hot rolling temperature. The results show that increasing cooling rate of ingots from natural cooling the precipitation hardening is enhanced, with increases of 10% and 12.5 % on the yield stress and working life of the anodes respectively, and that a minimum of 45 days of ageing is necessary to reach stable conditions for the precipitation hardening, with precipitates formation as CaSn_3. The hot roll temperature as not significant effect on the precipitation hardening of the anodes.
机译:厚度为6 mm的Pb-0.07%Ca-1.3%Sn阳极用于铜电解沉积的合适屈服应力是通过变形和沉淀硬化工艺实现的,其使用寿命取决于该屈服应力。在这种意义上,本发明的目的是优化沉淀硬化,为此目的找到模具中阳极和热轧温度的最佳冷却条件。结果表明,自然冷却使铸锭的冷却速率增加,沉淀硬化得到增强,阳极的屈服应力和工作寿命分别增加10%和12.5%,并且至少需要45天的时效才能进行阳极老化。达到了沉淀硬化的稳定条件,沉淀形成为CaSn_3。热辊温度对阳极的沉淀硬化没有显着影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号