The tube failures took place frequently in the superheater of 2x600MW units in a power plant. According to the condition of tube failures, the mechanical property and microstructure on running and failed tubes were tested and evaluated. The chemical composition and structure phase of inner oxide scale and deposit inside of the tubes were examined. The fractured surfaces of failed tube samples were observed. And the material examination was performed for original tube steels SA213-T91 and SA213-T22. The results show that raw materials of SA213-T91 and SA213-T22 tube in superheater are qualified. Besides, the characteristics of the SA213-T91 and SA213-T22 tube failure are typical short-term overheated rupture. The rupture temperature is located between two phase Ac1 ~ Ac3 of the two steels. It is recognized that putting SA213-T22 tubes in operation under the condition of long-term over heating causes the rupture of SA213-T91 and SA213-T22.
机译:在发电厂中2x600MW机组的过热器中经常发生管子故障。根据试管失效的情况,对运行中和失效的试管进行了力学性能和显微组织的测试和评估。检查管内部的氧化皮和沉积物的化学组成和结构相。观察失败的试管样品的断裂表面。然后对原始钢管SA213-T91和SA213-T22进行了材料检查。结果表明,过热器SA213-T91和SA213-T22的原料合格。此外,SA213-T91和SA213-T22管的故障特征是典型的短期过热破裂。断裂温度位于两种钢的两相Ac1〜Ac3之间。公认的是,在长期过热的条件下操作SA213-T22管会导致SA213-T91和SA213-T22破裂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号