The present invention discloses a method for preparing iron ore concentrates by recycling copper smelting slag tailings, and belongs to the technical field of metallurgy and tailings recycling. In the present invention, copper slag tailings obtained after copper pyrometallurgy and flotation and water are used as raw materials, and low-concentration sulfur dioxide flue gas is used as a leaching agent for leaching of metals such as iron, zinc, copper, arsenic, and silicon in the slag tailings; the leachate is purified step by step through processes such as replacement by metal iron powder and sulfide precipitation control, to separate zinc, copper, arsenic, etc.; a purified solution is mainly composed of FeSO4 or can be used for producing a ferric salt flocculant; obtained tailings are used to obtain iron ore concentrates through magnetic separation, and the obtained iron ore concentrates can be used for further producing ultra-pure iron ore concentrates.
机译:本发明公开了一种铜冶炼渣尾矿回收制备铁精矿的方法,属于冶金及尾矿回收技术领域。本发明以铜火法冶炼、浮选后获得的铜渣尾矿和水为原料,以低浓度二氧化硫烟气为浸出剂,浸出渣尾矿中的铁、锌、铜、砷、硅等金属;渗滤液通过金属铁粉置换、硫化物沉淀控制等过程逐步净化,分离锌、铜、砷等。;纯化溶液主要由FeSO4组成,或可用于生产铁盐絮凝剂;所得尾矿用于磁选获得铁精矿,所得铁精矿可用于进一步生产超纯铁精矿。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号