EXTRACTION METHOD OF IRON-ORE CONCENTRATE FROM AGED ALLUVIAL TAILINGS OF WET MAGNETIC SEPARATION OF IRON ORES OF SKARN-MAGNETITE TYPE

机译:从陈旧磁铁矿型磁铁矿湿法磁选老矿冲积渣中提取铁精矿的方法

摘要

FIELD: mining.;SUBSTANCE: method involves drying of tailing massif, identification of an outline of supergene-converted horizon, separation of thickness of tailings into non-productive lean tailings from upper part of technogenic massives, which are not subject to supergene changes, and productive gothite-magnetite-hematite horizons formed during supergene conversion of technogenic mineral raw material, removal of upper non-productive horizons, extraction of gothite-magnetite-hematite horizon and its processing so that iron-ore concentrate is obtained. Iron-ore concentrate with total iron content of more than 60% is obtained by means of a gravitation-and-magnetic or magnetic method from gothite-magnetite-hematite horizon saturated with iron, which is formed in thickness of aged tailings.;EFFECT: improving efficiency of complex development of iron-ore deposits and processing of wastes of iron-ore production; reducing anthropogenic load onto ecosystems.;2 cl, 2 tbl, 2 ex
机译:领域:采矿;物质:方法包括干燥尾矿地块,确定超基因转换层的轮廓,将尾矿的厚度从技术性块状物的上部分离成非生产性的精矿尾矿,这些均不受表观基因变化的影响,在生产成矿矿物原料的超基因转化,去除上部非生产层,提取针铁矿-磁铁矿-赤铁矿层及其加工过程中形成了生产性的针铁矿-磁铁矿-赤铁矿层,从而获得铁矿石精矿。总铁含量超过60%的铁矿石精矿是通过重力和磁法或磁法从充满铁的针铁矿-磁铁矿-赤铁矿层中得到的,该铁矿精矿形成于老化的尾矿的厚度中;效果:提高铁矿床综合开发效率和铁矿石生产废料处理效率;减少人类对生态系统的负担。; 2 cl,2 tbl,2 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号