首页> 外国专利> FOERFARANDE FOER BEHANDLING AV MOLYBDENHALTIGA NICKEL JAERN OCH SVAVEL INNEHAOLLANDE METALLSTENAR MELLANPRODUKTER OCH RESTER

FOERFARANDE FOER BEHANDLING AV MOLYBDENHALTIGA NICKEL JAERN OCH SVAVEL INNEHAOLLANDE METALLSTENAR MELLANPRODUKTER OCH RESTER

机译:含钼镍铁和硫的金属中间体及残渣的处理方法

摘要

1319503 Removal of Mo from Ni-containing residues SHERRITT GORDON MINES Ltd 16 Nov 1970 [7 Jan 1970 18 Sept 1970] 54459/70 Heading C1A Molybdenum is removed from residues containing Ni, Fe and S and possibly Cu, Co, Cr or W by mixing with the latter, before and/or during pelletizing of the same using water, an alkali in an amount equivalent to a residue-to- NaOH weight ratio of from 20 : 1 to 3 : 1; roasting the pellets at 540‹-870‹C. with a source of oxygen (e.g. air or steam) present to convert substantially all of the Mo into watersoluble alkali metal molybdates; quenching the roasted, pelletized mixture in water and agitating the slurry to extract and dissolve the molybdates; and finally separating the solution from the Ni-containing residue. Tungsten, if present in the original residue, may also be removed as water-soluble tungstates. The alkali to be used is preferably NaOH, KOH, Na 2 CO 3 , K 2 CO 3 or Na 2 S or mixtures of these.
机译:1319503从含镍残渣中去除钼SHERRITT GORDON MINES Ltd 1970年11月16日[1970年1月7日,1970年9月18日] 54459/70标题C1A从含镍,铁和硫以及可能的铜,钴,铬或钨的残渣中去除了钼在用水制粒之前和/或期间与后者混合,碱的量等于残渣与NaOH的重量比为20:1至3:1;在540℃-870℃下烘烤颗粒。存在氧源(例如空气或蒸汽)以将基本上所有的Mo转化为水溶性碱金属钼酸盐;在水中淬火烤制的颗粒状混合物,搅拌浆液以提取和溶解钼酸盐;最后从含镍残渣中分离溶液。如果原始残留物中存在钨,也可以将钨作为水溶性钨酸盐去除。所使用的碱优选为NaOH,KOH,Na 2 CO 3,K 2 CO 3或Na 2 S或它们的混合物。

著录项

获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号