Improved Method for producing Grain oriented Silicon Steel and Silicon Steel Products manufactured with the thus obtained

机译:制备晶粒取向硅钢的改进方法以及由此获得的硅钢产品

摘要

GRAIN-ORIENTED SILICON STEEL AND PROCESSING THEREFOR A process for producing grain-oriented silicon steel, and the steel produced thereby. The process includes the steps of: preparing a melt of silicon steel; casting the steel; hot rolling the steel; cold rolling the steel; decarburizing the steel; final texture annealing the steel; coating the steel with an aqueous solution comprised of from 4 to 30% phosphate ion, up to 6% magnesium ion, 5 to 34% colloidal silica and 0.15 to 6% hexavalent chromium; and curing the coated steel at a temperature of at least 1200.degree.F.
机译:取向硅钢及其加工生产取向硅钢的方法,以及由此生产的钢。该过程包括以下步骤:准备硅钢水;铸钢;热轧钢;冷轧钢;使钢脱碳;钢的最终织构退火;用由4至30%的磷酸根离子,至多6%的镁离子,5至34%的胶体二氧化硅和0.15至6%的六价铬组成的水溶液涂覆钢。并在至少1200°F的温度下固化涂层钢。

著录项

  • 公开/公告号AR212966A1

    专利类型

  • 公开/公告日1978-11-30

    原文格式PDF

  • 申请/专利权人 ALLEGHENY LUDLUM IND INC;

    申请/专利号AR19760263349

  • 发明设计人

    申请日1976-05-20

  • 分类号C22C38/02;

  • 国家 AR

  • 入库时间 2022-08-22 20:54:05

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号