COPOLYMER OF POLY (4,7-DIOXADECAMETHYLENE ADIPAMIDE)-PLYCAPROLACTAM CONTAINING TEREPHTHALIC ACID RESIDUES
展开▼
机译:含有对苯二甲酸残基的聚(4,7-二氧十二烯亚乙基酰胺)-聚己内酰胺的共聚物
展开▼
页面导航
摘要
著录项
相似文献
摘要
Method of producing copolymers intended to make fibers, particularly to produce poly (4,7-dioxadecamelitenadipamide) -policaprolactam copolymers, containing terephthalic acid, characterized in that it comprises: a) jointly incorporating salts of ** (Formula 01) ** b) heating the salts to form a random copolymer; and c) jointly incorporating the random copolymer and the polycaprolactam in fusion at a temperature comprised between the highest of its melting points and the lowest of its decomposition temperatures, such being the relationship between the temperature of joint fusion incorporation and the time during which applies to avoid the formation of random sequences and a copolymer having a molecular weight of about 5,000-100,000 and the following repetitive structural formula is formed: ** (Formula 02) ** in which X is within the range from about 97% by weight to about 87% by weight of the bivalent radical of - (CH2) 4- and the remainder is paraphenylene; y = 4-200 z = 4-200. (Machine-translation by Google Translate, not legally binding)
展开▼
机译:用于制备纤维的共聚物的制备方法,特别是用于制备包含对苯二甲酸的聚(4,7-二氧杂癸二烯酰胺)-聚己内酰胺共聚物的方法,其特征在于,该方法包括:a)共同掺入**(式01)**的盐b)加热盐以形成无规共聚物; c)在熔点最高和分解温度最低之间的温度下,将无规共聚物和聚己内酰胺共同掺入熔融状态,这是联合熔融掺入温度与所用时间之间的关系。避免形成随机序列,并形成分子量为约5,000-100,000的共聚物,并形成以下重复结构式:**(式02)**其中X的含量在约97%至约90%的范围内-(CH 2)4-的二价基团的重量为87%,其余为对亚苯基; y = 4-200 z = 4-200。 (通过Google翻译进行机器翻译,没有法律约束力)
展开▼