首页> 外国专利> Tinning appts. for copper, tin, bronze or nickel wires - has an acid etch bath, a tin (alloy) bath and a nozzle to remove excess metal

Tinning appts. for copper, tin, bronze or nickel wires - has an acid etch bath, a tin (alloy) bath and a nozzle to remove excess metal

机译:镀锡用于铜,锡,青铜或镍线-具有酸蚀液,锡(合金)液和喷嘴以去除多余的金属

摘要

In an appts. for thick tinning of Cu, Sn, Bronze or Ni lead wires of circuits and components, the wire is passes in turn through an acid etch bath, a tin(alloy)bath, with a first guide pulley, a wave shaped nozzle to wipe off surplus metal, and a cooling region with a broad guide pulley. The guide roll in the tin (alloy)bath has a protective coating of silicon nitride. It is further provided with stainless steel reinforcement. Thermal shock resistance is good at 20-350 degrees C (dipping pulley into the tin bath). The surface is not wetted by molten tin (alloy), the material has good mechanical strength, even under impact loading, exhibits low friction at 20-350 degrees C when immersed and when in air, low wear, low thermal expansion.
机译:在一个appts。为了对电路和组件的Cu,Sn,Bronze或Ni引线进行较厚的镀锡,将电线依次通过酸蚀浴,锡(合金)浴,第一导轮,波形喷嘴以擦去多余的金属,以及带有宽导轮的冷却区域。锡(合金)浴中的导辊具有氮化硅保护层。它进一步配备有不锈钢加强件。在20-350摄氏度(将滑轮浸入锡槽)中,耐热冲击性良好。表面不会被熔融的锡(合金)弄湿,即使在冲击载荷下,该材料也具有良好的机械强度,当浸入水中和在空气中时,在20-350摄氏度时表现出低摩擦,低磨损,低热膨胀。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号