ASSEMBLING AND MAGNETIZING METHOD FOR MAGNETIC CIRCUIT

机译:磁路的组装和充磁方法

摘要

PURPOSE:To enable to perform a complete magnetization in a weak magnetic field by a method wherein, in the assembled body of the magnetic circuit formed by providing a permanent magnet having R (at least a kind of rare-earth element containing Y), B and Fe as main ingredients, the permanent magnet is magnetized maintaining the specified range of high temperature. CONSTITUTION:An Fe-B-R permanent magnet consists of main ingredient of R of 8-30atm%, B of 2-28atm% and Fe of 42-90atm%, and its main phase consists of a pressure crystal phase, and Nd and Pr are used as R. A magnetizer has a plurality of magnetic poles whereon an electromagnetic coil 5 is wound around, a magnetic circuit consisting of an Fe-B-R magnet 1, a yoke 2 and a center pole 3 is provided thereon, and a high temperature is maintained in a high-temperature furnace within the temperature range of 50-140 deg.C, and the Fe- B-R magnet 1 is magnetized by applying a current to the magnetizer. As the above is assembled and magnetized in the high temperature atmosphere of 140 deg.C or below, the stabilization of heat ageing and the magnetization can be accomplished in one process.
机译:用途:通过以下方法能够在弱磁场中完成磁化:在通过提供具有R(至少一种含Y的稀土元素)的永磁体而形成的磁路的组装体中,B以铁为主要成分,永磁体被磁化,保持规定的高温范围。组成:Fe-BR永磁体的主要成分为R为8-30atm%,B为2-28atm%和Fe为42-90atm%,其主要相由压晶相组成,Nd和Pr为充磁机具有多个磁极,电磁线圈5缠绕在磁极上,并在其上设置由Fe-BR磁铁1,磁轭2和中心极3组成的磁路,并且将Fe-BR磁体1保持在50-140℃温度范围内的高温炉中,并且通过向磁化器施加电流来使Fe-BR磁体1磁化。当在140℃或更低的高温气氛中组装并磁化以上内容时,可以在一个过程中完成热老化和磁化的稳定化。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号