METHOD FOR CONTINUOUSLY CASTING AL-LI ALLOY

机译:连续铸造铝锂合金的方法

摘要

PURPOSE:To restrain the development of shrinkage hole and to improve the productivity by executing injection or projection of solid grains at the time of cooling a cast billet drawn from a mold. CONSTITUTION:Molten metal supplied from a nozzle 1 is cooled in the mold 3 circulating cooling water through an inlet 4 and outlet 5 and the solidification is started to make the cast billet 10, and the cast billet is continuously drawn downward. At the exposed place of the cast billet 10 from the mold 3, blasting material injected with pressurized gas of air, etc., from an injection nozzle 8 or projected with impeller 9 is collided to the cast billet 10 to cool the cast billet 10. By this method, the solid-liquid coexisting zone is shortened and the development of the shrinkage hole in the cast billet can be restrained. Further, the casting speed can be increased and even if break out happens, possibility of explosion is eliminated.
机译:目的:通过在冷却从模具中拉出的铸坯时执行固体颗粒的注入或喷射,来限制缩孔的产生并提高生产率。组成:从喷嘴1供给的熔融金属在模具3中冷却,使冷却水通过入口4和出口5循环,并开始凝固以制造铸坯10,并将铸坯连续向下拉。在铸坯10从模具3露出的地方,从喷射喷嘴8喷射或用叶轮9喷射的空气等的加压气体的喷砂材料与铸坯10碰撞,以冷却铸坯10。通过这种方法,缩短了固液共存区域,并且可以抑制铸坯中缩孔的发展。此外,可以提高铸造速度,并且即使发生破裂,也消除了爆炸的可能性。

著录项

  • 公开/公告号JPH01233051A

    专利类型

  • 公开/公告日1989-09-18

    原文格式PDF

  • 申请/专利权人 SUMITOMO LIGHT METAL IND LTD;

    申请/专利号JP19880056290

  • 发明设计人 OKA KAZUYOSHI;OSONO TOMOYA;

    申请日1988-03-11

  • 分类号B22D11/00;B22D11/04;B22D11/041;B22D11/049;B22D11/124;

  • 国家 JP

  • 入库时间 2022-08-22 06:46:36

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号