The invention can be used in metallurgy in the production of low alloy mild steel. SUMMARY: The minimum amount of niobium microalloying for a suit is determined depending on the total carbon content, sulfur and phosphorus in the melt according to the formula: (% Nb) 0,04 + I (% C), (% S), (% P) 8K. where (% Nb) - minimum number of niobium microalloying required is for, in weight%: 1% C {) {5%) (% P) - the total content of carbon, sulfur and phosphorus in the melt before deoxidation.%;. By - experienced coefficient taking into account the absorption of niobium equal 0,85-0.95.
机译:本发明可用于冶金中低合金低碳钢的生产。概述:西装的最小铌微合金化量取决于熔体中的总碳含量,硫和磷,其计算公式如下:(%Nb)0.04 + I(%C),(%S), (%P)8K。其中(%Nb)-所需的最小铌微合金化数量,以重量%计:1%C {){5%)(%P)-脱氧前熔体中碳,硫和磷的总含量。%; 。经验系数考虑了铌的吸收,等于0.85-0.95。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号