PURPOSE: To reduce a rise of inner resistance a positive electrode layer at the time of discharge and supply high working voltage for providing a small- sized and light-weight thermal cell in relation to a positive electrode active material for a thermal cell, in which a positive electrode active material of a lithium iron disulfide thermal cell is improved, as well as its manufacturing method and a thermal cell using it. ;CONSTITUTION: A starting material is to be an iron powder, or a powder, at least whose surface is an iron oxide or iron hydroxide, a metallic iridium powder and sulphor. A positive electrode active material for a thermal cell consisting of a composite compound of iron disulphide and iridium disulphide having an iridium content ratio 5 to 20wt.% is manufactured through a process of mixing the starting material, a process of heating and synthesizing its mixture at a temperature 350 to 500°C and a process of crushing an obtained composite.;COPYRIGHT: (C)1993,JPO&Japio
机译:用途:为了减少内层电阻在放电时的升高,并提供高工作电压,以提供一种相对于热电池用正极活性材料而言小巧轻便的热电池,其中改进了二硫化锂铁热电池的正极活性材料及其制造方法和使用它的热电池。 ;组成:原料应为铁粉或至少表面为氧化铁或氢氧化铁,金属铱粉和硫磺的粉。通过混合起始原料,加热并合成其混合物的步骤,制造由铱含量比为5至20wt。%的由二硫化铁和二硫化铱的复合化合物组成的热电池用正极活性材料。在350至500℃的温度下进行和粉碎所得复合材料的过程。;版权所有:(C)1993,日本特许厅&日本apio

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号