Nonwovens of synthetic continuous filaments obtained by melt extrusion, in which at least 50% of the filaments contain at least from 0, 5 to 3%, preferably from 0.6 to 1.5%, of a polyorganosiloxane introduced into the said filaments during their manufacture.PP Process for the manufacture of these nonwovens, in which, before extrusion of the polymer melt to produce the filaments by flowing through orifices of a die, a silicone oil of polyorganosiloxane type is introduced in the proportion at least of 0,5 to 3%, preferably from 0.6 to 1.5% relative to the polymer, into the melt of the latter.P PThe polyorganosiloxane product employed is of the polydiorganosiloxane type with a molecular weight of between 1,000 and 250,000, preferably between 7,500 and 70,000, corresponding to dynamic viscosities of 50 to 10,000 mPa s; stable under extrusion conditions. PPUse of the nonwovens, chiefly as a support for floor coverings with stitched pile.
机译:通过熔融挤出获得的合成连续长丝的非织造布,其中至少50%的长丝包含至少0%,5%至3%,优选0.6%至1.5%的聚有机硅氧烷在制造过程中引入到所述长丝中。 P>

这些无纺布的制造方法,其中,在将聚合物熔体挤出以通过流经模头的孔口而生产长丝之前,以至少0的比例引入聚有机硅氧烷类型的硅油,相对于聚合物的熔体为5至3%,优选为0.6至1.5%。所使用的聚有机硅氧烷产物是聚二有机硅氧烷类型的,分子量为1,000至250,000,优选为1至250,000。 7,500和70,000,对应于50至10,000 mPa s的动态粘度;在挤出条件下稳定。

非织造布的用途,主要用作缝制绒头的地板覆盖物的支撑。