首页> 外国专利> A METHOD FOR PRODUCING A REDUCED CHROMIUM-ORE BEARING POWDER

A METHOD FOR PRODUCING A REDUCED CHROMIUM-ORE BEARING POWDER

机译:一种生产还原铬铬矿粉的方法

摘要

PCT No. PCT/JP89/00256 Sec. 371 Date Nov. 13, 1989 Sec. 102(e) Date Nov. 13, 1989 PCT Filed Mar. 9, 1989 PCT Pub. No. WO89/08724 PCT Pub. Date Sep. 21, 1989.A reduced chromium-ore bearing powder used for production of a chromium-containing steel in a converter, is produced by a reduction of chromium ore-powder having a particle-diameter of 3 mm or less by a carbonaceous reducing agent having a particle diameter of 3 mm or less in an inert-gas atmosphere, while the chromium-ore powder and carbonaceous reducing agent are stirred and mixed with each other in the reaction chamber (5). The reduced chromium-ore powder has 3 mm or less of particle diameter. Acid-soluble chromium is in an amount of 85% or more of the total chromium, and acid-soluble iron is in an amount of 95% or more of the total iron.
机译:PCT号PCT / JP89 / 00256第二部分371日期1989年11月13日102(e)1989年11月13日PCT申请日期1989年3月9日PCT公开WO89 / 08724 PCT公开号1989年9月21日,一种还原剂,用于在转炉中生产含铬钢,用还原铬矿粉,是通过用碳素还原粒径为3mm或更小的铬矿粉而制得的在惰性气体气氛中,将粒径为3mm或更小的还原剂,同时在反应室(5)中搅拌并混合铬矿石粉末和含碳还原剂。还原的铬矿石粉末具有3mm或更小的粒径。酸溶性铬的含量为全部铬的85%以上,酸溶性铁的含量为全部铁的95%以上。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号