Low silica X (LSX) zeolites having a framework Si/Al ratio equal to 1. 0 with lithium exchange levels greater than a threshold level of 70% exhibit unexpectedly higher capacity for nitrogen adsorption compared to LSX-zeolite with lower lithium exchange levels. These materials provide high performance adsorbents for PSA air separation processes at a lower cost for the adsorbent because of the lower threshold lithium exchange levels compared to highly exchanged lithium X- zeolite known in the prior art.
机译:与锂交换水平较低的LSX沸石相比,骨架Si / Al比等于1. 0且锂交换水平大于阈值水平70%的低二氧化硅X(LSX)沸石具有出乎意料的更高的氮吸附能力。由于与现有技术中已知的高度交换的锂X-沸石相比阈值锂交换水平较低,因此这些材料以较低的吸附剂成本为PSA空气分离工艺提供了高性能的吸附剂。

著录项

  • 公开/公告号US5268023A

    专利类型

  • 公开/公告日1993-12-07

    原文格式PDF

  • 申请/专利权人 AIR PRODUCTS AND CHEMICALS INC.;

    申请/专利号US19920957532

  • 发明设计人 JOHN F. KIRNER;

    申请日1992-10-05

  • 分类号B01D53/04;

  • 国家 US

  • 入库时间 2022-08-22 04:32:33

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号