A typical aluminum alloy brazing material (A) disclosed comprises over 7.0 wt. % and not more than 12.0 wt. % of Si, over 0.1 wt. % and not more than 8.0 wt. % of Cu, over 0.05 wt. % and not more than 0.5 wt. % of Fe, further at least one kind selected from a group consisting of over 0.5 wt. % and not more than 5.5 wt. % of Zn, over 0.002 wt. % and not more than 0.3 wt. % of In and over 0.002 wt. % and not more than 0.3 wt. % of Sn, and the balance of Al and inevitable impurities. A typical aluminum alloy brazing sheet with a three-layer structure cladded comprises a brazing material (A), a core material (B) comprising over 0.6 wt. % and not more than 2.5 wt. % of Si, over 0.5 wt. % and not more than 2.5 wt. % of Cu, over 0.05 wt. % and not more than 2.0 wt. % of Mn, and the balance of Al and inevitable impurities, and a sacrificial material comprising at least one kind selected from a group consisting of over 0.5 wt. % and not more than 6.0 wt. % of Zn, over 0.002 wt. % and not more than 0.3 wt. % of In and over 0.002 wt. % and not more than 0.3 wt. % of Sn, and the balance of Al and inevitable impurities, or comprises a core material (B) cladded both sides thereof with the brazing material (A). By using the inventive brazing materials or brazing sheets, the brazing heating can be performed at a IMAGE
机译:所公开的典型的铝合金钎焊材料(A)占7.0重量%以上。 %和不大于12.0重量%。超过0.1 wt。%的Si %和不大于8.0 wt。超过0.05 wt。 %且不大于0.5重量%。铁,优选至少0.5重量%的铁,还选自0.5重量%以上的铁。 %且不大于5.5wt。%。超过0.002 wt。 %和不大于0.3重量%。大于或等于0.002 wt。 %和不大于0.3重量%。 %的锡,以及余量的铝和不可避免的杂质。典型的覆有三层结构的铝合金钎焊板包括钎焊材料(A),芯材(B),其含量超过0.6wt。%。 %且不大于2.5重量%。 0.5重量%以上的Si的%。 %且不大于2.5重量%。超过0.05 wt。 %且不大于2.0 wt。牺牲材料,其包含至少0.5重量%的Mn,以及Al和不可避免的杂质的余量,以及牺牲材料,所述牺牲材料包括选自0.5重量%以上的至少一种。 %和不大于6.0 wt。超过0.002 wt。 %和不大于0.3重量%。大于或等于0.002 wt。 %和不大于0.3重量%。 %的Sn,以及余量的Al和不可避免的杂质,或者包括芯材料(B),在芯材料的两侧覆盖有钎焊材料(A)。通过使用本发明的钎焊材料或钎焊片,可以在<图像>下进行钎焊加热。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号