In order to produce thin strip strips with high cast strip toughness from thin strip cast strips of Cr-stainless steel containing Nb, Ti and Al in an amount of 0.05% or more, the process is characterized in that the steel contains 13-25% by weight of Cr, 0.05 to 1% by weight of one or more of Ti, Al and V, 0.03% by weight or less of C, 0.03% by weight or less of N, and 0.3-3% Or less Casting a thin sheet cast strip of Cr-stainless steel, having a p-value of 10 mm or less; Hot-rolling the thin sheet strip at a reduction rate of 5-50% at a temperature of 1150-950C to form a thin strip; At a temperature of 1150-950C, the thin strip is cooled slowly at a rate of 20C / sec or less, or 5 seconds or more of the thin strip is left; RTI ID = 0.0 700 C /RTI ;P (%) = 420C + 470N + 23Ni + 9Cu + 7Mn-11.5Cr-11.5Si-12Mo-23V-47Nb-49Ti-52Al + 189
机译:为了从含有0.05%以上的Nb,Ti和Al的Cr不锈钢薄带铸钢带制造高铸带韧性的薄带钢,其特征在于,所述钢的含量为13%至25%。 Cr的重量百分比,Ti,Al和V中的一种或多种的重量百分比为0.05-1%,C的重量百分比等于或小于0.03%,N的重量百分比等于或小于0.03%,N的重量百分比等于或小于0.3-3% p值小于或等于10mm的Cr不锈钢薄板铸造带;在1150-950℃的温度下以5-50%的压下率热轧薄板条,形成薄条;在1150-1950℃的温度下,以20℃/秒以下的速度缓慢地冷却薄带,或者留下5秒以上的薄带。 700℃; P(%)= 420C + 470N + 23Ni + 9Cu + 7Mn-11.5Cr-11.5Si-12Mo-23V-47Nb-49Ti-52Al + 189

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号