High temp. material contains sintered magnesia (MgO) particles in integrated configuration and a mineral phase of magnesium orthotitanate (Mg2TiO4) lying between the magnesia particles. Also claimed is a process (I) for mfg. a high temp. material with a mineral phase of Mg2TiO4 lying between sintered MgO particles in integrated configuration, the process being novel in that coarse MgO particles are uniformly mixed with fine titania (TiO2) particles and the mixt. fired. Further claimed is a process (II) for mfg. the above material, novel in that a mixt. of MgO and TiO2 is fired to form a primary sintered mass, which is pulverised to form fine particles, which are added to coarse MgO particles and the coarse to average size MgO particles, and the mixt. is heated to carry out secondary sintering to form the high temp. material. Also claimed is a further process (III) for mfg. a high temp. material with a mineral phase of Mg2TiO4 which lies between sintered MgO particles in integrated configuration, novel in that coarse MgO particles are uniformly mixed with fine Mg2TiO4 particles and the mixt. is sintered.
机译:高温该材料包含一体构造的烧结氧化镁(MgO)颗粒和位于氧化镁颗粒之间的原钛酸镁(Mg2TiO4)矿物相。还要求保护一种制造方法(I)。高温这种材料具有Mg2TiO4的矿物相处于一体构造的烧结MgO颗粒之间,该过程是新颖的,因为粗MgO颗粒与细的二氧化钛(TiO2)颗粒和混合物均匀混合。被解雇。进一步要求保护的是制造方法(II)。以上材料,新颖之处在于混搭。烧成MgO和TiO 2,形成初级烧结块,将其粉碎形成细颗粒,将其加入粗MgO颗粒和粗至平均粒度的MgO颗粒中,并混合。加热以进行二次烧结以形成高温。材料。还要求保护一种进一步的制造方法(III)。高温矿物相为Mg2TiO4的矿物相处于一体构造的烧结MgO颗粒之间,其新颖之处在于粗MgO颗粒与细Mg2TiO4颗粒和混合物均匀混合。被烧结。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号