首页> 外国专利> PROCEDURE FOR WELDING BY INTERMEDIATE CASTING OF FINELY PERLITIZED LANES.

PROCEDURE FOR WELDING BY INTERMEDIATE CASTING OF FINELY PERLITIZED LANES.

机译:精细浇铸车道的中间铸造焊接工艺。

摘要

THE INVENTION REFERS TO A PROCEDURE FOR THE WELDING OF INTERMEDIATE MELTING OF RAILS WITH A FINE PERLITICAL STRUCTURE THROUGH A STEEL POINT GENERATED ALUMINOTHERMICALLY IN ONE OF THE FOUNDRY MOLDS SURROUNDING BOTH END OF THE RAIL. AFTER WELD COOLING, THE WELDING SURFACE AREA AND HEAT INFLUENCED ZONES ARE HEATED NEARLY FROM THE UPPER ZONE BY MEANS OF A SCHOCK TYPE BURNER DURING A SPACE OF TIME FROM 50 TO 150 SECONDS. THE BURNER FEEDS RESPECTIVELY WITH AT LEAST 10,000 L / HOUR OF OXYGEN AND 3,500 L / HOUR OF PROPANE OR ACETYLENE, THE COMBUSTION SURFACE OF THE BURNER HEAD IS POSITIONED AT A DISTANCE FROM THE SURFACE OF PASSAGE OF WELDING AND ZONES OF INFLUENCE OF WARMING, IN A CORRESPONDING VALUE IN MILLIMETERS MEASURED OF 0.1 RESPONSIBLE TO THE MEASURED WEIGHT OF THE RAIL USED, MEASURED IN KG.
机译:本发明涉及一种通过在钢的两端围绕的一个铸模中以铝热化学方式产生的钢点,对具有精细的蠕变结构的钢进行中间熔化的焊接方法。焊接冷却后,在50到150秒的时间间隔内,通过SCHOCK型燃烧器,几乎从上部区域加热了焊接表面区域和受热影响区域。燃烧器的进料分别为至少10,000 L / h的氧气和3,500 L / h的丙烷或乙炔,燃烧器头部的燃烧表面与焊接通道和加热影响区的距离相距不远,对应于所用铁轨的测量重量(以千克为单位)的以毫米计的对应值是0.1。

著录项

  • 公开/公告号ES2095106T3

    专利类型

  • 公开/公告日1997-02-01

    原文格式PDF

  • 申请/专利权人 ELEKTRO-THERMIT GMBH;

    申请/专利号ES19940108205T

  • 发明设计人 KUSTER FRANK DR.;

    申请日1994-05-28

  • 分类号B23K23/00;E01B11/52;

  • 国家 ES

  • 入库时间 2022-08-22 03:24:04

获取专利

客服邮箱:kefu@zhangqiaokeyan.com