首页> 外国专利> WEIGHT LOS FINISHING METHOD OF POLYESTER TEXTILE FABRIC

WEIGHT LOS FINISHING METHOD OF POLYESTER TEXTILE FABRIC

机译:涤纶纺织面料的重量损失整理方法

摘要

An interlaced polyester yarn 90 denier/60 filament produced by an interlacing MGY 50denier/36filament and a hish shrinkage(ISD) 40 denier/24 filament is twisted to S twist 1200 TPM and is used as a warp, Sd 150 denier/48 filament which is given 1800 TPM in the ratio of S:Z=2:2 is used as a weft. The flat fabric made of this warp and weft. And the flat fabric made of this warp and weft is relaxed in 130 degree C for 10minutes in anion scouring agent 0.5/l and soda ash 1.0/l by the liquid ratio of 10-20:1, and pre-dyed in 98 degree C* 55m/min, and preset in 180 degree C*65m/min and a polyester fabric which has no warp line and no feeling, is processed with decreasing.
机译:由交织的MGY 50旦尼尔/ 36根细丝和his收缩率(ISD)40旦尼尔/ 24根细丝生产的交织聚酯纱线90旦尼尔/ 60根细丝被捻成S捻1200 TPM,并用作经纱,Sd 150旦尼尔/ 48根细丝,以S:Z = 2:2的比率给出1800TPM用作纬纱。由这种经纱和纬纱制成的扁平织物。然后,将这种经纬线制成的扁平织物在阴离子精练剂0.5 / l和纯碱1.0 / l中在130摄氏度下以10-20:1的液体比率松弛10分钟,并在98摄氏度下进行染色。 * 55m / min,以180℃×65m / min的预设值进行加工,使无翘曲,无手感的聚酯纤维减少。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号