首页> 外国专利> A MAGNETIC CERAMIC COMPOSITION FOR MICROWAVE DEVICE, A MAGNETIC CERAMIC FOR MICROWAVE DEVICES THEREFROM AND A PREPARATION METHOD THEREOF

A MAGNETIC CERAMIC COMPOSITION FOR MICROWAVE DEVICE, A MAGNETIC CERAMIC FOR MICROWAVE DEVICES THEREFROM AND A PREPARATION METHOD THEREOF

机译:用于微波装置的磁陶瓷组合物,用于微波器件的磁陶瓷及其制备方法

摘要

The present invention relates to a material for a microwave band part used in electronic devices for civil and industrial use, which is easy to control saturation magnetization and has a low ferrimagnetic resonance half width and a good Curie temperature, a microwave element And a method for producing the same.;The magnetic ceramic composition for a microwave device according to the present invention comprises a yttrium oxide, a ferric oxide, a tin oxide, an aluminum oxide, and a calcium source as main components and is represented by the following composition formula. The magnetic ceramic for a microwave device according to the present invention is characterized by the following composition formula , Yttrium oxide, iron oxide, tin oxide, aluminum oxide, and calcium carbonate (or calcium oxide), followed by molding and sintering. The resulting product has a saturation magnetization of 100 to 1,800 G and a saturation magnetization of 3 G / A temperature coefficient and a ferrimagnetic resonance half width of 60 Oe or less:;Y 3-x Ca x Sn x Fe 5-y Al y O 12;Here, 0.1? X? 1 and 0.2? Y? 1.5.
机译:微波元件及其制造方法,微波元件及其制造方法本发明的微波装置用磁性陶瓷组合物以氧化钇,三氧化二铁,氧化锡,氧化铝和钙源为主要成分,由以下组成式表示。根据本发明的用于微波装置的磁性陶瓷的特征在于以下组成式:氧化钇,氧化铁,氧化锡,氧化铝和碳酸钙(或氧化钙),然后成型并烧结。所得产品的饱和磁化强度为100至1,800 G,饱和磁化强度为3 G / A,温度系数和亚铁磁共振半峰宽为60 Oe或更小:; Y 3-x Ca x Sn x Fe 5-y Al y O 12 ;这里0.1? X? 1和0.2?是啊1.5。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号