The invention sulfide - relates to a method of manufacturing a cadmium (CdS) film, a sulfide prepared by the CBD method-cadmium (CdS) thin film chloride-and large dense amount of cadmium (CdCl 2) heat treatment by determining the surface also flat The present invention relates to a method for producing a cadmium sulfide (CdS) thin film. The substrate is cleaned, a cadmium sulfide (CdS) thin film is prepared using the CBD method, and the cadmium sulfide (CdS) thin film is manufactured by using a cadmium chloride (CdCl) film. 2 ) Put it in a specially made carbon boat with a solution or cadmium chloride (CdCl 2 ) powder and cadmium sulfide (CdS) powder and heat-process it for 3 to 10 minutes at high temperature in an inert gas atmosphere such as argon or nitrogen. Chemical-bath-deposition (CBD) method and chloride-carbide, which are characterized by manufacturing a cadmium sulfide (CdS) crystal having a large, dense and flat surface, and producing a highly efficient solar cell. CdS thin film and method for producing a cadmium sulfide (CdS) thin film by heat treatment with cadmium (CdCl 2 ).
机译:硫化物-本发明涉及一种制造镉(CdS)膜的方法,一种通过CBD方法制备的硫化物-氯化镉(CdS)薄膜-以及大量致密的镉(CdCl 2)通过确定表面也平坦来进行热处理技术领域本发明涉及一种用于生产硫化镉(CdS)薄膜的方法。清洁基板,使用CBD方法制备硫化镉(CdS)薄膜,并通过使用氯化镉(CdCl)薄膜制造硫化镉(CdS)薄膜。 2 )将其与溶液或氯化镉(CdCl 2 )粉末和硫化镉(CdS)粉末一起放入特制的碳舟中,并进行3到3次热处理。在惰性气体如氩气或氮气中,在高温下放置10分钟。化学浴沉积(CBD)方法和碳化物碳化物,其特征在于制造具有大,致密且平坦的表面的硫化镉(CdS)晶体,并生产高效的太阳能电池。 CdS薄膜和通过用镉(CdCl 2 )进行热处理生产硫化镉(CdS)薄膜的方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号