This invention concerns a method of reducing the gaping values of railway tracks made of steel to less than 3.6 mm. It is characteristic of this invention that the rolled and leveled rails are heated briefly, i. e., for approx. 10 to 25 sec, until reaching a maximum temperature of 100. degree. C. in the rail head and a maximum of 260° C. in the web, and then they are allowed to cool again immediately.
机译:本发明涉及一种将钢制轨道的间隙值减小到小于3.6mm的方法。本发明的特征在于,将被轧平的钢轨短暂地加热,即,将其加热。 e。,大约10至25秒,直到达到最高温度100度。轨头中的温度为C.,腹板中的最高温度为260°C,然后让它们立即再次冷却。