(57) Abstract With electrodeposition method, per 1l approximately the nickel of 0.034 - approximately 0.047 mols, per 1l approximately the tungsten of 0.15 - approximately 0.28 mols, per 1l approximately per hydroxy carboxylic acid, and 1l of 0.13 - approximately 0.43 mols 0 mols or from the electrodeposition bath which approximately includes the boron of 0.077 - approximately 0.15 mols in melting state nickel - tungsten content tunic is formed on the base substance. PH of electrodeposition bath is approximately 6 - approximately 9, electrodeposition desirably is done at the temperature of approximately 100F - approximately 140F.
机译:(57)<摘要>通过电沉积方法,每1升约镍为0.034-约0.047摩尔,每1升约钨为0.15-约0.28摩尔,每1升约为每羟基羧酸,以及1升0.13-约0.43摩尔在基础物质上形成0摩尔或从电沉积浴中形成的熔融态镍-钨含量的外衣,该电沉积浴大约包含0.077-约0.15摩尔的硼。电沉积浴的PH约为6-约9,电沉积最好在约100F-约140F的温度下进行。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号