首页> 外国专利> METHOD FOR PREVENTING BELT-LIKE UNEVEN BRIGHTNESS OF COLD-ROLLED AUSTENITIC STAINLESS STEEL STRIP

METHOD FOR PREVENTING BELT-LIKE UNEVEN BRIGHTNESS OF COLD-ROLLED AUSTENITIC STAINLESS STEEL STRIP

机译:防止冷轧奥氏体不锈钢带的带状不均匀亮度的方法

摘要

PROBLEM TO BE SOLVED: To easily and stably prevent the occurrence of belt-like uneven brightness in a cold-rolled, annealed, and pickled steel strip of austenitic stainless steel. ;SOLUTION: In the method for preventing the belt-like uneven brightness of the cold-rolled austenitic stainless steel strip, austenitic stainless steel in which the value of A(γ) represented by A(γ)=30×(C+N)+0.5×Mn+Ni-1.3×Cr+11.8 is made to +1.8, e.g. SUS304 or SUS304L of -1.6 to +1.6 A(γ) is hot-rolled, coiled at 300-600°C, and then subjected to steps of annealing and pickling, cold rolling, finish annealing and pickling by ordinary method. In particular, it is desirable to apply, before coiling, forced cooling where the amount of cooling water is controlled to regulate a rise in coil temperature owing to recuperation after coiling so that the coil temperature does not exceed 600°C.;COPYRIGHT: (C)2003,JPO
机译:要解决的问题:为了轻松稳定地防止在奥氏体不锈钢冷轧,退火和酸洗钢带中出现带状亮度不均。 ;解决方案:在防止冷轧奥氏体不锈钢带的带状亮度不均的方法中,奥氏体不锈钢中,A(γ)的值由A(γ)= 30×(C + N)+ 0.5×Mn + Ni-1.3×Cr + 11.8为<+1.8,例如将-1.6至+ 1.6A(γ)的SUS304或SUS304L热轧,在300-600℃下卷取,然后通过普通方法进行退火和酸洗,冷轧,精整退火和酸洗的步骤。特别地,期望在卷取之前施加强制冷却,其中控制冷却水的量以调节由于卷取后的回热而引起的卷取温度的升高,使得卷取温度不超过600℃。 C)2003年,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号