THERMOSTABLE COMPOSITE BASED ON SILOXANE BLOCK-COPOLYMER

机译:基于硅氧烷嵌段共聚物的热固性复合材料

摘要

FIELD: polymers, organosilicon compounds. SUBSTANCE: invention describes thermostable composite based on siloxane block-copolymer comprising mineral filling agent, antistructurizing addition and vulcanizing agent that comprises block-copolymer consisting of inflexible phenylsesquioxane block of the following structure: where m = 2-3 and flexible block dimethylphenylsiloxane oligomer of the following structure: where n = 20-30; a, b = from 0 to 30 mole% in the mole ratio of flexible and rigid blocks = 1-2 and diphenylguanidine is used as vulcanizing agent and components are taken in the following ratio, weight p. p.: siloxane block-copolymer, 100.0; mineral filling agent, 27-32; antistructurizing addition, 8-10; vulcanizing agent, 1.5-2.0. Invention provides enhancement of thermal stability of composite up to 450-500 C and development thicken materials on their base working in the range of temperature from 60 to 500 C. EFFECT: valuable properties of composite. 2 cl, 2 tbl
机译:领域:聚合物,有机硅化合物。物质:本发明描述了基于硅氧烷嵌段共聚物的热稳定复合材料,所述硅氧烷嵌段共聚物包含矿物填充剂,抗结构化添加剂和硫化剂,所述硫化剂包含由以下结构的柔性苯倍半氧烷嵌段组成的嵌段共聚物:<图像文件=“ 00000003.GIF” he =“ 33 “ id =” imag00000003“ imgContent =” undefined“ imgFormat =” GIF“ wi =” 39“ />其中m = 2-3且具有以下结构的柔性嵌段二甲基苯基硅氧烷低聚物:其中n = 20-30; a,b = 0至30摩尔%,以柔性和刚性嵌段的摩尔比= 1-2,并且使用二苯基胍作为硫化剂,并且以以下重量比p取组分。 p .:硅氧烷嵌段共聚物,100.0;矿物填充剂,27-32;抗结构化加成,8-10;硫化剂1.5-2.0。本发明增强了复合材料在高达450-500℃的热稳定性,并且在60℃至500℃的温度范围内在其基础上开发增稠材料。效果:复合材料的有价值的性能。 2厘升,2汤匙

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号