PROBLEM TO BE SOLVED: To prepare a liquid crystal polyester solution having a better productivity, a manufacturing process therefor and a liquid crystal polyester film having a better productivity.;SOLUTION: The liquid crystal polyester solution is obtained by dissolving 0.5-100 pts.wt. of a liquid crystal polyester in 100 pts.wt. of a solvent described below in an atmosphere with an oxygen concentration of ≤5% at a temperature of ≥140°C and ≤200°C. The manufacturing process for the liquid crystal polyester solution comprises dissolving 0.5-100 pts.wt. of the liquid crystal polyester in 100 pts.wt. of a solvent described below in an atmosphere with the oxygen concentration of ≤5% at the temperature of ≥140°C and ≤200°C. The solvent contains a halogen-substituted phenolic compound expressed by formula (I) (wherein, A is a halogen atom or a trihalogenated methyl group; (i) is an integer of 1-5; and when (i) is ≥2, A's may be different from each other or the same).;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:为了制备具有更高生产率的液晶聚酯溶液,其制备方法和具有更高生产率的液晶聚酯膜。解决方案:通过溶解0.5-100pts.wt获得液晶聚酯溶液。 。重量为100 pts.wt的液晶聚酯在温度为140℃至200℃的氧气浓度为5%的气氛中,加入以下所述溶剂。液晶聚酯溶液的制造方法包括溶解0.5-100pts.wt。 100 pts.wt.的液晶聚酯含量在温度为140℃和200℃的氧气浓度为5%的气氛中,加入以下所述溶剂。溶剂包含由式(I)表示的卤素取代的酚类化合物(其中,A是卤素原子或三卤代甲基;(i)是1-5的整数;并且当(i)是≥ 2时, A可能彼此不同或相同)。;版权:(C)2006,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号