Method to overcome instability of ultra-shallow semiconductor junctions
Method to overcome instability of ultra-shallow semiconductor junctions
展开▼
机译:克服超浅半导体结不稳定性的方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
A method of forming a stable unction on a microelectronic structure on a semiconductor wafer having a silicon surface layer on a substrate includes the following steps: implanting dopant ions into the surface layer; cleaning and oxidizing the surface layer, and twice annealing the wafer to recover a damaged silicon crystal structure of the surface layer resulting from the low energy ion implantation. The first annealing process uses a temperature range of 800° C. to 1200° C. for a duration from about a fraction of a second to less than about 1000 seconds, with a ramp-up rate of about 50° C./second to about 1000° C./second. The second annealing process uses a temperature range of 400° C. to 650° C. for a time period of from about 1 second to about 10 hours, and more preferably, from about 60 seconds to about 1 hour. Both annealing processes include cooling processes.
展开▼