A heat treatment process of serpentine as raw material for mineral carbonation is provided to efficiently remove -OH groups existing in untreated serpentine and improve crystalline property of the treated serpentine by heat-treating milled serpentine powder at a desired temperature for a constant time period. The heat treatment process comprises the steps of: milling serpentine ore as raw material of mineral carbonation into powder with particle size less than 125 micrometers; heating the powder at above 700deg.C for more than 10 minutes under oxygen or atmosphere; and cooling the powder to ambient temperature. Time for heat treatment of serpentine is more than 10 minutes at a constant heat treatment temperature excluding temperature raising process. The serpentine ore typically includes metal elements such as silicon, magnesium, iron, calcium, aluminum, etc.
机译:提供了蛇纹石作为用于矿物碳酸化的原料的热处理工艺,以通过将碾磨的蛇纹石粉末在期望的温度下恒定时间段进行热处理来有效地去除未处理的蛇纹石中存在的-OH基团并改善经处理的蛇纹石的结晶性质。热处理工艺包括以下步骤:将蛇纹石矿石作为矿物碳酸化的原料,研磨成粒径小于125微米的粉末。在氧气或气氛下,于700℃以上将粉末加热10分钟以上。并将粉末冷却至环境温度。在不考虑升温过程的情况下,在恒定的热处理温度下,蛇纹石的热处理时间超过10分钟。蛇纹石矿石通常包含金属元素,例如硅,镁,铁,钙,铝等。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号