摘要

PROBLEM TO BE SOLVED: To provide a carbon fiber structure having improved oxidation resistance, generating little fine powder and exhibiting high metal-supporting characteristics, a method for the production of the structure and an oxidized fiber for the production method. ;SOLUTION: The objective carbon fiber structure having an oxidation resistance of ≥620°C, a fine power generation of ≤18 mg/g and a metal supporting property of ≥550 ppm is produced by forming an oxidized fiber structure from a polyacrylonitrile-based oxidized fiber having an ash content of ≤0.1 wt.%, a zinc content of 100-500 ppm, a phosphorus content of 20-250 ppm, an iron content of 0.5-10 ppm and a calcium content of 5-60 ppm (in terms of weight) and carbonizing the oxidized fiber structure in an inert gas at ≥1,700°C. The specific gravity of the polyacrylonitrile-based oxidized fiber is preferably 1.33-1.45.;COPYRIGHT: (C)2001,JPO
机译:解决的问题:为了提供一种具有改善的抗氧化性,几乎不产生细粉并显示出高的金属负载特性的碳纤维结构,该结构的制造方法以及用于该制造方法的氧化纤维。 ;解决方案:通过由碳纳米管形成氧化纤维结构,可生产具有620℃的抗氧化性,18毫克/克的精细发电量和550 ppm的金属支撑性能的目标碳纤维结构。聚丙烯腈基氧化纤维,其灰分含量≤0.1wt。%,锌含量为100-500 ppm,磷含量为20-250 ppm,铁含量为0.5-10 ppm,钙含量为5- 60ppm(以重量计)并在1,700℃的惰性气体中将氧化的纤维结构碳化。聚丙烯腈基氧化纤维的比重优选为1.33-1.45 。;版权所有:(C)2001,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号