VITRIFIED GRINDING STONE AND ITS MANUFACTURING METHOD, AND METHOD FOR GRINDING CAST IRON WORKPIECE USING THE SAME GRINDING TOOL

机译:陶瓷粉磨石及其制造方法,以及使用相同粉磨工具磨铸铁工件的方法

摘要

PROBLEM TO BE SOLVED: To provide a vitrified grinding stone having a long service life, even under a high load condition, and its manufacturing method, and a method for grinding a cast iron workpiece using the grinding stone.;SOLUTION: In this vitrified grinding stone 10, a degree of concentration of super-abrasive grain 12 is 160 to 185, a volume ratio of aggregate 14 is 3 to 10 volume%, a particle size is #170 to #270, a difference of a particle diameter between a minimum particle and a maximum particle is within 0.014 mm, and glassy bonding agent 16 having a softening point ≥550°C occupies 25 to 35 volume%. When the cast iron workpiece is ground by using the vitrified grinding tool 10, grinding efficiency is set at 120 to 200 mm3/mm× second, and peripheral speed of the vitrified grinding tool 10 and the cast iron workpiece is set at ≥100 m/second.;COPYRIGHT: (C)2007,JPO&INPIT
机译:解决的问题:提供即使在高负荷条件下使用寿命长的玻璃化磨石及其制造方法,以及使用该磨石磨铸铁工件的方法。石材10,超级磨料颗粒12的浓缩度为160至185,骨料14的体积比为3至10体积%,粒径为#170至#270,最小粒径之间的差颗粒和最大颗粒在0.014mm以内,软化点为550℃的玻璃状粘合剂16占25-35体积%。使用玻璃化磨具10对铸铁工件进行磨削时,磨削效率为120〜200mm 3 / mm×。其次,将玻璃化磨削工具10和铸铁工件的圆周速度设定为100m /秒。版权所有:(C)2007,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号