FIELD: production of items from high-doped high-temperature wrought nickel alloys for disks of gas-turbine engines.;SUBSTANCE: proposed method includes vacuum induction melting for obtaining ingot for deformation. At least one cycle of pre-extrusion is performed which is followed by recrystallization annealing. Extrusion of blank is performed in die by repeated forcing of blank from cylindrical to taper part of die at temperature below Tc.d.γ' by 55-95C. Die is heated to temperature not below Tc.d.γ' -250C and not above the blank heating temperature. Rate of deformation , where Tc.d.γ' is temperature of complete dissolving of γ' phase. During each subsequent stage of forcing-out the blank, direction of forcing out is reversed as compared with previous stage. Prior to final deformation, blank is subjected to intermediate annealing. Items made from high-temperature nickel alloy have homogeneous structure in complex stampings and stable level of properties ensuring reduction of extrusion force and final deformation.;EFFECT: enhanced efficiency; increased factor of utilization of metal.;7 cl, 1 dwg, 3 tbl, 6 ex
机译:领域:用高掺杂的高温锻造镍合金生产燃气轮机盘用的物品。物质:所提出的方法包括真空感应熔炼以获得变形的铸锭。进行至少一个预挤出循环,然后进行重结晶退火。坯料的挤出是通过在低于Tc.d.γ的温度下55-95℃下反复将坯料从圆柱体压到模头的锥形部分中而进行的。模具被加热至不低于T -250℃且不高于空白加热温度的温度。变形率,其中T cd&gamma;'< / sub>是γ完全溶解的温度。相。在每个后续的坯料挤出阶段,与前一阶段相比,挤出的方向相反。在最终变形之前,对毛坯进行中间退火。用高温镍合​​金制成的物品在复杂的冲压件中具有均匀的结构,并且性能水平稳定,可确保减少挤压力和最终变形。增加金属利用率。; 7 cl,1 dwg,3 tbl,6 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号