BASE MATERIAL WATERPROOF CONSTRUCTION METHOD, STRUCTURE BY THIS CONSTRUCTION METHOD AND PRIMER FOR ADHESIVE LAYER USED FOR THIS CONSTRUCTION METHOD

机译:基体材料防水施工方法,该施工方法的结构以及用于该施工方法的粘结层的底漆

摘要

PROBLEM TO BE SOLVED: To provide a composite structure and its construction method for further improving adhesive strength of a waterproof material and an asphalt pavement material.;SOLUTION: The base material waterproof construction method is a construction method of the composite structure composed of at least a base material, the waterproof material and the asphalt pavement material. The waterproof material is constructed on the base material, and hydraulic setting alumina powder and/or hydraulic setting hauynite-based mineral powder are rolled on a surface of the waterproof material, by laying a hot asphalt pavement material on an adhesive layer surface, by forming an adhesive layer, after solidifying a curing primer up to at least a dry-to-touch (JIS K-5400) state, by applying the curing primer of including 10 to 500 pts.wt. to a curing resin of 100 pts.wt. in an application quantity of 100 to 1000 (g/m2).;COPYRIGHT: (C)2008,JPO&INPIT
机译:解决的问题:提供一种用于进一步提高防水材料与沥青路面材料的粘合强度的复合结构及其施工方法。解决方案:基材防水施工方法是至少由以下组成的复合结构的施工方法:基础材料,防水材料和沥青路面材料。通过在基材上构造防水材料,并通过将热沥青路面材料铺设在粘合剂层表面上,通过将水硬性氧化铝粉末和/或水硬性硅藻土基矿物粉末辊压在防水材料的表面上,来形成防水材料。通过施加包括10至500pts.wt。%的固化底漆,使固化底漆固化至至少干摸(JIS K-5400)状态后,形成粘合剂层。到100 pts.wt的固化树脂。施用量为100至1000(g / m 2 )。;版权所有:(C)2008,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号