PPROBLEM TO BE SOLVED: To provide a compound structure improved in the bonding strength of a water-proof material and an asphalt paving material, and a construction method for it. PSOLUTION: According to this waterproof construction method for a base material, in a construction method of the compound structure composed of at least the base material, the water-proof material and the asphalt paving material, the water-proof material is constructed on the base material, a curable primer containing 10 to 500 wt. parts water-setting alumina powder and/or water-setting hauynite mineral powder to 100 wt. parts curable resin is coated on the surface of the water-proof material in a coating amount of 100 to 1,000 (g/mSP2/SP), and after the curable primer is solidified at least to the state of set-to-touch (JIS K-5400), an adhesive layer is formed, and the thermal asphalt paving material is laid on the surface of the adhesive layer and subjected to rolling compaction. PCOPYRIGHT: (C)2004,JPO
机译:<解决的问题:提供一种提高防水材料与沥青铺路材料的粘结强度的复合结构及其施工方法。

解决方案:根据该用于基材的防水施工方法,在至少由基材,防水材料和沥青铺路材料组成的复合结构的施工方法中,构造防水材料在基础材料上,包含10至500 wt。将水定型氧化铝粉末和/或水定型硅藻土矿物粉末分批至100 wt。将部分可固化树脂以100到1,000(g / m 2 )的涂覆量涂覆在防水材料的表面上,并在可固化底漆固化后至少固化至凝固状态触摸(JIS K-5400),形成粘合剂层,并且将热沥青铺路材料铺设在粘合剂层的表面上并进行压实。

版权:(C)2004,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号