机译:低钙铝合金的制造方法及低钙铝合金的铸锭

摘要

PROBLEM TO BE SOLVED: To provide a process for manufacturing an Al alloy containing little Ca, which inexpensively and reliably reduces Ca, and to provide an Al alloy base metal applicable to the manufacturing process.;SOLUTION: The process manufactures the Al alloy containing as little Ca as 0.002 mass% or less. The process comprises a base-metal-melting step S1 for melting a base metal of an Al alloy which contains 0.003 mass% or more Ca together with 1 mass% or less Mg, a molten-metal-holding step S2 for reducing a Ca content to 0.002 mass% or less by exposing the surface of the molten metal obtained in the base-metal-melting step S1 to atmospheric air for 20 minutes or longer, and a pouring step S3 of pouring the molten metal into a mold having a desired shape. The base metal of the Al alloy to be used preferably contains 0.2 mass% or less Mg. After the molten-metal-holding step S2, a Mg addition step of adding a desired amount of Mg to the molten metal is preferably performed.;COPYRIGHT: (C)2005,JPO&NCIPI
机译:解决的问题:提供一种制造含钙少的铝合金的方法,该方法廉价且可靠地还原钙,并提供适用于该制造方法的铝合金贱金属。 Ca为0.002质量%以下。该方法包括:使包含0.003质量%以上的Ca和1质量%以下的Mg的铝合金的贱金属熔融的贱金属熔融步骤S1,和降低Ca含量的熔融金属保持步骤S2。通过将在贱金属熔化步骤S1中获得的熔融金属的表面在大气中暴露20分钟或更长时间,以及将熔融金属倒入具有期望形状的模具中的倒出步骤S3,将其减少到0.002质量%以下。 。所使用的Al合金的基础金属优选含有0.2质量%以下的Mg。在熔融金属保持步骤S2之后,优选地执行向熔融金属中添加期望量的Mg的Mg添加步骤。版权所有:(C)2005,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号