首页> 外国专利> Lead material null mass for the loom reed which becomes making use of the Cr stainless steel wire or the steel wire and the said steel wire for abrasion proof it is superior corrosion-resistant and

Lead material null mass for the loom reed which becomes making use of the Cr stainless steel wire or the steel wire and the said steel wire for abrasion proof it is superior corrosion-resistant and

机译:利用Cr不锈钢丝或钢丝以及用于耐磨性的所述钢丝制成的织机簧片的铅材料无效质量,具有优异的耐腐蚀性和

摘要

PROBLEM TO BE SOLVED: To enhance the total cost performance of a wear resistant component by improving the corrosion resistance, cold workability and wear resistance of a Cr based stainless steel wire rod or steel wire.;SOLUTION: The Cr based stainless steel wire rod or steel wire has a composition comprising, by mass, 0.05 to 0.30% C, 0.05 to 2.0% Si, 0.1 to 1.5% Mn, 12 to 17.5% Cr, 0.05 to 3.0% Mo and 0.01 to 0.15% N, further comprising one or more kinds selected from 0.05 to 1.0% Nb, 0.05 to 1.0% Ti and 0.05 to 1.0% V, and satisfying the conditions that PI value by formula (A) is ≥14.0 and CI value by formula (B) is 3 to 20, and comprises carbonitride (carbide+nitride) of 1 to 8% by the total content in the matrix composed of a ferritic structure: PI value=Cr+3Mo-17C-7N (A), and CI value=(V+Ti+Nb)/C (B).;COPYRIGHT: (C)2006,JPO&NCIPI
机译:要解决的问题:通过改善Cr基不锈钢盘条或钢丝的耐腐蚀性,冷加工性和耐磨性来提高耐磨部件的总成本性能。解决方案:Cr基不锈钢盘条或钢丝的组成包含按质量计0.05%至0.30%的C,0.05%至2.0%的Si,0.1%至1.5%的Mn,12%至17.5%的Cr,0.05%至3.0%的Mo以及0.01%至0.15%的N,进一步包括从0.05至1.0%的Nb,0.05至1.0%的Ti和0.05至1.0%的V中选择更多的种类,并且满足以下条件:式(A)的PI值为≥ 14.0并且式(B)的CI值为3至20 ,并且在由铁素体结构组成的基质中的总含量中包含1%至8%的碳氮化物(碳化物+氮化物):PI值= Cr + 3Mo-17C-7N(A),CI值=(V + Ti + Nb)/ C(B).;版权所有:(C)2006,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号