METHOD FOR PREPARING ZSM-5 ZEOLITE USING CRYSTALLINE NANO-SIZED ZSM-5 NUCLEUS, CAPABLE OF OBTAINING UNIFORM ZSM-5 ZEOLITE WITHOUT IMPURITIES

机译:用结晶纳米尺寸的ZSM-5核制备ZSM-5沸石的方法,能够获得均匀的ZSM-5沸石

摘要

PURPOSE: A method for preparing ZSM-5 zeolite is provided to control the crystal size of ZSM-5 zeolite by varying the size of crystalline nano-sized ZSM-5 nucleus.;CONSTITUTION: A method for preparing ZSM-5 zeolite includes a nucleus preparing process, a reaction mixture preparing process, and a crystallizing process. In the nucleus preparing process, the size of ZSM-5 nucleus is between 70 and 300nm. In the reaction mixture preparing process, the ZSM-5 nucleus is added in a base liquid to obtain a reaction mixture. The base liquid includes water glass silica source, alumina source, a neutralizing agent, and water. The mixture is crystallized at temperature between 150 and 200 degrees Celsius.;COPYRIGHT KIPO 2011
机译:目的:提供一种制备ZSM-5沸石的方法,以通过改变晶体纳米ZSM-5晶核的大小来控制ZSM-5沸石的晶体大小。;组成:一种制备ZSM-5沸石的方法包括一个核制备过程,反应混合物制备过程和结晶过程。在原子核制备过程中,ZSM-5原子核的大小在70至300nm之间。在反应混合物的制备过程中,将ZSM-5核添加到基础液体中以获得反应混合物。基础液包括水玻璃二氧化硅源,氧化铝源,中和剂和水。混合物在150到200摄氏度之间结晶。; COPYRIGHT KIPO 2011

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号