PURPOSE: A finishing material composition capable of using as a surface protector of a concrete structure is provided to protect the surface of concrete from various deterioration factors using the swelling property of bentonite. CONSTITUTION: A finishing material composition capable of using as a surface protector of a concrete structure, using a ladle slag crystal-growing reaction contains 10~30wt% of cement, 20~50wt% of silica or limestone powder, 20~50wt% of powder additive including ladle slag and granulated blast furnace slag in a ratio of 2~5:10~40; 1~3wt% of anhydrous gypsum, 2~7wt% of ethylene vinyl acetate polymer powder, 3~10wt% of bentonite powder, and 1~3wt% of sodium carbonate. The composition additionally contains 1~8wt% of inorganic pigment.
机译:用途:提供一种能够用作混凝土结构表面保护剂的饰面材料组合物,以利用膨润土的溶胀性保护混凝土表面免受各种劣化因素的影响。组成:一种可以用作混凝土结构表面保护剂的饰面材料组合物,它通过使用钢包渣结晶生长反应而包含10〜30wt%的水泥,20〜50wt%的二氧化硅或石灰石粉,20〜50wt%的粉包括钢包渣和高炉矿渣的比例为2〜5:10〜40的添加剂; 1〜3wt%的无水石膏,2〜7wt%的乙烯醋酸乙烯酯聚合物粉末,3〜10wt%的膨润土粉和1〜3wt%的碳酸钠。该组合物还包含1〜8wt%的无机颜料。

著录项

  • 公开/公告号KR101046970B1

    专利类型

  • 公开/公告日2011-07-06

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20080123361

  • 发明设计人 김상현;천성민;조규용;

    申请日2008-12-05

  • 分类号C04B18/14;C04B14/10;C04B16/04;

  • 国家 KR

  • 入库时间 2022-08-21 17:50:05

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号